MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical GOYENCHEM-DF-04 LED Grade Optical Light Diffusion Scattering Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: adding GOYENCHEM-DF SERIES can also increase the transmittance of the optical for diffusion equally. It can be applied for various LED, CCFL or other materials that require diffuse and scattering properties.

Features:

  • Great light diffusion/ scattering effect
  • Three dimension web structure, fine powder that makes the particles can dispersion evenly and diffusion evenly
  • Processing ability
  • The gloss is better than traditional organic materials
  • As the replacement of the low end materials for better transmittance
  • Higher glossiness
  • Heat stabilizations
  • For the additive in the optical products
  • High compatibility
  • As the low glossiness adjustment agent in the plastic industry
Applications:
  • LED/LED TV Backlight
  • PC.PS.PMMA.PET.PVC.PP plastic
  • Diffusion film/board
  • Paint & coating, ink applications
  • packaging materials application
  • injection extrusion products Applications
  • LED Bulb Lamp
  • EPOXY Packaging Materials
  • Car industry
  • electrical and electronic material
  • Medical Equipment
  • packaging applications

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/cc
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49
 
Descriptive Properties
AppearanceFine Powder
Heat Resistant Temperature>300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN438 / 266746

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.