MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ 9100 CR Polycarbonate (PC) / Polyethylene Terephthalate (PET)  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Overview: EMERGE™ PC/PET 9100 CR advanced resin is a polycarbonate blend with excellent chemical resistance. This grade was designed for use in medical equipment housings and can withstand repeated exposure to a variety of cleaners and disinfectants commonly used in hospitals. This grade has good aesthetics and excellent toughness.

Applications:

  • Medical device housings or enclosures
  • UL Listing for HB

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0090 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0080 in/inASTM D955
Melt Flow 8.5 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 111
@Thickness 3.20 mm
Injection Molded; ASTM D785
Tensile Strength at Break 56.2 MPa
@Thickness 3.20 mm
50 mm/min, Injection Molded; ASTM D638
Tensile Strength, Yield 50.0 MPa
@Thickness 3.20 mm
50 mm/min, Injection Molded; ASTM D638
Elongation at Break 150 %
@Thickness 3.20 mm
50 mm/min, Injection Molded; ASTM D638
Elongation at Yield 4.7 %
@Thickness 3.20 mm
50 mm/min, Injection Molded; ASTM D638
Tensile Modulus 2210 MPa
@Thickness 3.20 mm
5 mm/min, Injection Molded; ASTM D638
Flexural Strength 77.2 MPa
@Thickness 3.20 mm
1.3 mm/min, Injection Molded; ASTM D790
Flexural Modulus 2100 MPa
@Thickness 3.20 mm
1.3 mm/min, Injection Molded; ASTM D790
Izod Impact, Notched 750 J/m
@Thickness 3.20 mm,
Temperature -30.0 °C
Injection Molded; ASTM D256
 950 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256
Dart Drop, Total Energy 46.3 J
@Thickness 3.20 mm,
Temperature 23.0 °C
Injection Molded, Peak Energy; ASTM D3763
 55.4 J
@Thickness 3.20 mm,
Temperature -40.0 °C
Injection Molded, Peak Energy; ASTM D3763
 63.3 J
@Thickness 3.20 mm,
Temperature 23.0 °C
Injection Molded, Total Energy; ASTM D3763
 80.2 J
@Thickness 3.20 mm,
Temperature -40.0 °C
Injection Molded, Total Energy; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 117 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.2 °CUnannealed; ASTM D648
Vicat Softening Point 144 °C
@Load 1.02 kg
Rate B (120°C/h); ASTM D1525
Flammability, UL94 HB
@Thickness 1.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 249 - 282 °C
Mold Temperature 43.3 - 65.6 °C
Drying Temperature 121 °C
Dry Time 3.00 - 4.00 hour

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo EMERGE™ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET)
Mitsubishi Iupilon® MB4405U PC/Polyester
Trinseo CALIBRE™ 200-10 Polycarbonate Resin
Aclo Acculoy POL062L Polycarbonate PET Alloy
Aluminum 6082-T6

PZZDWST060 / 142269

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.