MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ 200-23 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: CALIBRE™ 200-23 polycarbonate resins are produced in compliance with the US FDA and EU food contact regulations. They provide excellent impact resistance, heat distortion resistance and optical clarity. The CALIBRE™ 200-23 series products are available in 4 additive packages: CALIBRE 200: No mold release or UV Stabilizer. CALIBRE 201: Mold release. CALIBRE 202: UV Stabilizer. CALIBRE 203: Mold release and UV stabilizer. (Not that CALIBRE 202 and 203 grades are not available in Europe and do not comply with EU food contact regulations).

Applications:

  • Food processors
  • Beverage containers
  • Food utensils
  • Other packaging applications
Govt. and Industry Standards:
  • US FDA 21 CFR 177.1580
  • CSA
  • Underwriters Laboratory (UL)
  • EU food contact 2002/72/EC
Automotive Specifications:
    FORD ESF-M4D100-A1

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183/A
Water Absorption 0.15 %
@Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 0.32 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 in/inISO 294-4
Melt Flow 23 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 72ASTM D785
Hardness, Rockwell R 118ASTM D785
Tensile Strength at Break 65.5 MPa50 mm/min; ASTM D638
 66.0 MPaISO 527-2/50
Tensile Strength, Yield 60.0 MPa50 mm/min; ASTM D638
 60.0 MPaISO 527-2/50
Elongation at Break 120 %50 mm/min; ASTM D638
 120 %ISO 527-2/50
Tensile Modulus 2300 MPaISO 527-2/50
 2340 MPa50 mm/min; ASTM D638
Flexural Strength 96.5 MPaMethod I (3 point load), 2.0 mm/min; ASTM D790
 97.0 MPa2.0 mm/min; ISO 178
Flexural Modulus 2400 MPa2.0 mm/min; ISO 178
 2410 MPaMethod I (3 point load), 2.0 mm/min; ASTM D790
Izod Impact, Notched 750 J/mASTM D256
Izod Impact, Notched (ISO) 74.0 kJ/m²ISO 180/A
Izod Impact, Unnotched (ISO) NBISO 180
Tensile Impact Strength 378 kJ/m²ASTM D1822
Dart Drop, Total Energy 72.3 J3.39 m/sec; ASTM D3763
Abrasion 45[%], Taber; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+17 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmASTM D149
Dissipation Factor 0.0010
@Frequency 50 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 250 V
@Thickness 2.00 mm
Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
ASTM D696
Hot Ball Pressure Test 125 °CIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 139 °CUnannealed; ISO 75-2/B
 142 °CAnnealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 126 °CUnannealed; ASTM D648
 126 °CAnnealed; ISO 75-2/A
 136 °CAnnealed; ASTM D648
Vicat Softening Point 147 °CISO 306/B50
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
Oxygen Index 26 %ISO 4589-2
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ISO 489
Haze <= 1.0 %ASTM D1003
Transmission, Visible 89 %ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ IM 401-11 Polycarbonate Resin
Mocom (ALBIS) ALTECH® PC-HT A 1000/500 High Heat Polycarbonate
Trinseo CALIBRE™ 200-10 Polycarbonate Resin
Trinseo CALIBRE™ 200-6 Polycarbonate Resin
Trinseo CALIBRE™ 7100-15 Polycarbonate

PDWST002 / 142211

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.