MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Process Technologies Inc Tyfluor™ 1000 Sanitary Gasket
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Tyfluor 1000 is a chemically modified version of PTFE that provides much improved sealing capabilities while maintaining the property characteristics consistent with virgin PTFE material. Tyfluor's chemical inertness and extremely low level extractables combined with its superior stress relaxation and low deformation characteristics make it an ideal gasket and seal material for the pharmaceutical and biotechnology industries. Clamp gaskets made from Tyfluor 1000 provide a much higher level of performance when compared to conventional PTFE products used in pharmaceutical and hygienic applications. They also perform better in applications with frequent thermal cycling or vibration. Tyfluor gaskets prevent intrusion into pipe fittings and do not create issues related to flow restrictions or cross contamination. The broad capabilities of Tyfluor gaskets allows for gasket inventory reduction. Tyfluor 1000 is FDA and USP Class VI (toxicity) compliant

Information provided by Process Technologies Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.18 g/ccASTM D1457
Deformation 3.2 %
@Pressure 138 MPa,
Temperature 26.0 °C
ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 5000 psiASTM D1457
Elongation at Break 450 %ASTM D1457
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
Minimum Service Temperature, Air -128 °C
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
ColorWhite
Compatibility for ChemicalsAcetoneExcellent
 AmmoniaExcellent
 Hydrochloric AcidExcellent
 Hydrofluoric AcidExcellent
 Hydrogen PeroxideExcellent
 Isopropyl AlcoholExcellent
 Nitric AcidExcellent
 Phosphoric AcidExcellent
 Sodium HydroxideExcellent
 Sodium HypochloriteExcellent
 Steam to 400ºF (204ºC)Limited
 Sulfuric AcidExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Process Technologies Inc Sanifluor® 1000 Formulated Aflas® Elastomer

PPTI02 / 138114

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.