MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nexeo® HIVAL® 5303 High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Features:
  • BPA Free Food Contact
  • Acceptable
Agency Ratings: FDA 21 CFR 177.1640

RoHS Compliance: RoHS Compliant

Forms: Pellets

Processing:

  • Method Extrusion
  • Injection Molding

Information provided by Nexeo® Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D1505
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 94ASTM D785
Tensile Strength, Yield 4000 psiASTM D638
Tensile Modulus 280000 psiASTM D638
Flexural Modulus 280000 psiASTM D790
Izod Impact, Notched 3.00 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 195 °FASTM D648
Vicat Softening Point 200 °FASTM D1525
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 390 - 450 °FInjection Molding
Middle Barrel Temperature 400 - 450 °FInjection Molding
Front Barrel Temperature 425 - 500 °FInjection Molding
Nozzle Temperature 425 - 500 °FInjection Molding
Zone 1 380 - 440 °FExtrusion
Zone 3 390 - 450 °FExtrusion
Zone 5 400 - 470 °FExtrusion
Die Temperature 410 - 450 °FExtrusion
Melt Temperature 425 - 525 °FInjection Molding
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Global GP-110 High Impact Polystyrene
Alcoa KAMA 3000 High Impact Polystyrene (HIPS)
NIZHNEKAMSKNEFTEKHIM 825 High Impact Polystyrene
Versalis Edistir® PD ICE S 900 High Impact Polystyrene - Very High ESCR
Overview of materials for Polystyrene, Impact Modified

PNEXEO920 / 197604

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.