MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical 95HC SAN Resin  (discontinued **)
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include make-up cases and other products requiring chemical resistance

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccASTM D792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cmASTM D955
Melt Flow 3.4 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 32 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 124ASTM D785
Tensile Strength, Yield 80.0 MPa50 mm/min; ASTM D638
Elongation at Break 6.0 %50 mm/min; ASTM D638
Modulus of Elasticity 3.31 GPa50 mm/min; ASTM D638
Flexural Yield Strength 132 MPa50 mm/min; ASTM D790
Flexural Modulus 3.80 GPa15 mm/min; ASTM D790
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 120 - 180 secUL Rating PLC 5 (120-180 sec)
Comparative Tracking Index 400 - 600 VUL Rating PLC 1 (400-600 volts)
Hot Wire Ignition, HWI 15 - 30 secUL Rating PLC 3 (15-30 sec)
High Amp Arc Ignition, HAI >= 120 arcsUL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR <= 10.0 mm/minUL Rating PLC 0 (0-10 mm/min)
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
Vicat Softening Point 107 °C1000 g; ASTM D1525
Flammability, UL94 HB
@Thickness 1.59 mm
 HB
@Thickness 3.17 mm
Flame Spread 25.0 mm/min
@Thickness 3.17 mm
FH3

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance
LG Chemical 90HR SAN, High Transparency, Heat Resistance, Chemical Resistance
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance
LG Chemical 92HR SAN Resin

PLAZ96 / 50354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.