MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® L42009PE Film (Butene Grade) LLDPE
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: Linear Low Density Polyethylene Butene Copolymer for Film Extrusion

Formolene® L42009PE is a general-purpose film grade linear low density made using gas-phase technology. The resin exhibits excellent toughness and strength when drawn down to thin gauges.

Formolene® L42009PE meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Applications: Blending Resin, Industrial Liners, Industrial Packaging, Garment Bags and Co-Extrusion

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.919 g/ccASTM D1505
Thickness 0.984 mil
Melt Flow 0.95 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Condition E; ASTM D1238
Antiblock Level 1700 ppm
Slip Level 1350 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 690 %ASTM D882
Film Elongation at Break, TD 920 %ASTM D882
Elmendorf Tear Strength MD 150 gASTM D1922
Elmendorf Tear Strength TD 385 gASTM D1922
Dart Drop Test 135 gASTM D1709
Film Tensile Strength at Break, MD 5100 psiASTM D882
Film Tensile Strength at Break, TD 4130 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 20 %ASTM D1003
Gloss 40 %45°C; ASTM D523
 
Processing PropertiesOriginal ValueComments
Blow-up Ratio (BUR) 2.5
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin
ExxonMobil NTX™ NTX 095 Super Strength Film Resin
Formosa Plastics Formolene® L62009E2 Film (Hexene Grade) LLDPE
Total LLDPE LL 1820 H Linear Low Density Polyethylene - Blown Film
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film

PFPCPQ063 / 150295

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.