MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE FM-2669 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink FM-2669 is a general purpose thermoplastic elastomer, available in Nat, Blk, and colors, used in a variety of automotive interior applications, including automotive floor mats. Sarlink FM-2669 is a UV stabilized, medium hardness, high density, wear-resistant grade suitable for extrusion, injection molding or thermoforming.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Filled; Good Adhesion; Good Colorability; Good Processability; Good Toughness; High Density; Medium Hardness; High Specific Gravity; Low Flow; UV Resistant; Wear Resistant

Uses: Automotive Applications; Automotive Interior Parts; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion; Thermoforming

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183
Melt Flow 0.10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74
@Time 15.0 sec
Injection Molded; ISO 868
 75
@Time 5.00 sec
Injection Molded; ISO 868
 79
@Time 1.00 sec
Injection Molded; ISO 868
Tensile Strength at Break 870 psiISO 37
Elongation at Break 500 %ISO 37
 
Processing PropertiesOriginal ValueComments
Processing Temperature 440 - 480 °FMelt, Injection
Rear Barrel Temperature 440 - 480 °FInjection
Middle Barrel Temperature 440 - 480 °FInjection
Front Barrel Temperature 440 - 480 °FInjection
Nozzle Temperature 440 - 480 °FInjection
Zone 1 420 - 460 °FExtrusion
Zone 2 420 - 460 °FExtrusion
Zone 3 420 - 460 °FExtrusion
Zone 4 420 - 460 °FExtrusion
Zone 5 420 - 460 °FExtrusion
Die Temperature 420 - 460 °FExtrusion
Mold Temperature 60.0 - 90.0 °FInjection
Injection Pressure 200 - 1000 psiInjection
Back Pressure 25.0 - 125 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 120 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Colors Available
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1047 / 237538

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.