MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 354.0-T61, Permanent Mold Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 354.0-T61; UNS A03540; AA354.0-T61; Al354.0-T61
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.71 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 48.0 ksiAA
Tensile Strength, Yield >= 37.0 ksi
@Strain 0.2 %
AA
Elongation at Break >= 3.0 %AA; in 2 in. (50 mm) or 4D
Tensile Modulus 73.1 GPa
Compressive Yield Strength 250 MPaClass 1 or 10; Class 2 is higher, class 12 is lower
Compressive Modulus 74.5 GPa
Poissons Ratio 0.33Calculated Value
Fatigue Strength 135 MPa
@# of Cycles 5.00e+8
Notch Status unknown, R.R. Moore Test
 345 MPa
@# of Cycles 10000
Notch Status unknown, R.R. Moore Test
Machinability 30 %0-100 Scale (100=best)
Shear Modulus 27.6 GPa
Shear Strength 199 MPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000540 ohm-cmAA; Typical 32% IACS Conductivity
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 389 J/gTypical for cast aluminum
CTE, linear 11.6 µin/in-°F
@Temperature 20.0 - 100 °C
AA; Typical
 12.7 µin/in-°F
@Temperature 20.0 - 300 °C
AA; Typical; average over range
Specific Heat Capacity 0.963 J/g-°C
Thermal Conductivity 0.300 cal cm/sec-cm²-°CAA; Typical at 25°C
Melting Point 1000 - 1105 °FAA; Typical
Solidus 1000 °FAA; Typical
Liquidus 1105 °FAA; Typical
 
Processing PropertiesOriginal ValueComments
Solution Temperature 980 °Fhold at temperature 10 - 12 hrs; quench in hot water 140 to 176°F
Aging Temperature 310 °Fhold at temperature 10 - 12 hrs
 310 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 87.2 - 89.4 %As remainder
Copper, Cu 1.6 - 2.0 %
Iron, Fe <= 0.20 %
Magnesium, Mg 0.40 - 0.60 %
Manganese, Mn <= 0.10 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si 8.6 - 9.4 %
Titanium, Ti <= 0.20 %
Zinc, Zn <= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 354.0-T62, Permanent Mold Cast
354.1 Aluminum Composition Spec
Aluminum A380.0-F Die Casting Alloy
Aluminum A356.0-T61, Permanent Mold Cast
Aluminum 357.0-T6, Permanent Mold Cast

MAC3540T61 / 9899

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.