MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Lacqtene® 1003 FE 30 HDPE, blow molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Molded

Material Notes: Medium density radical polyethylene made by high tubular pressure process for medical applications requiring sterilization : small and medium stiff containers for parental mixtures, ophthalmic solutions, sterilized ampoules.

Advised temperature profile : 150 to 180°C

Lacqtène 1003FE30 is easily converted on aseptical machines. (Rommelag or similar)

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.928 g/ccISO 1183
Melt Flow 0.30 g/10 minISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 16.0 MPaISO 527
Elongation at Break 550 %ISO 527
Modulus of Elasticity 0.350 GPaISO 527-2
Dart Drop Test 150 g50µ; ISO 7765-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 117 °CISO 11357-3
Vicat Softening Point 106 °CISO 306
 
Optical PropertiesOriginal ValueComments
Haze 10 %
@Thickness 0.0500 mm
ASTM D 1003
 
Descriptive Properties
Food StatusComplies with the French and European pharmacopeas.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total MDPE 3802 Medium Density Polyethylene, Blow Molding
Total Lumicene® mPE M 3509 Medium Density Polyethylene, Blow Molding
Petroquimica Triunfo Trithene® SX 9003 MDPE - Blow Molding
Aclo Accutech Polyethylene HD0234G30UVL High Density Glass Reinforced UV Stabilized
Amco PRIMATOP MDPE 003937 Medium Density Polyethylene

PFINAP076 / 38659

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.