MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cathay Terryl® PA56T Renewable Engineering Polyamide Fiber
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Derived from plant sugars. Provides high performance, good processability, dyeability, and intrinsic flame resistance.

Information provided by Cathay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Absorption <= 0.300 %
Relative Viscosity 2.5 - 3.2 cP
 
Thermal PropertiesOriginal ValueComments
Melting Point 269 °C
 
Optical PropertiesOriginal ValueComments
Yellow Index <= 15 %
 
Descriptive Properties
Amine Terminal Group40-60 mmol/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cathay Terryl® PA56 Renewable Engineering Polyamide Fiber
Cathay Terryl® PA510 Renewable Engineering Polyamide Fiber
Cathay PA56 Renewable Engineering Polyamide, DAM
Cathay PA56 Renewable Engineering Polyamide, 50% RH
Cathay PA510 Renewable Engineering Polyamide

PCATH021 / 217617

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.