MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Xantar® 18 UR Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances where quality is a key requirement. The Xantar® range includes:
  • clear and tinted grades for transparent applications
  • reinforced materials
  • Flame retardant and halogen free types
  • lubricated materials for added wear resistance

Mitsubishi Engineering Plastics acquired the Xantar® product line from DSM in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Water Absorption 0.35 %Sim. to ISO 62
Viscosity Number 43 cm³/gLimiting Viscosity Number; ISO 1628-4
Linear Mold Shrinkage, Flow 0.0060 cm/cmISO 294-4
Melt Flow 27.6 g/10 min
@Load 1.20 kg,
Temperature 300 °C
Calculated from Volume Flow Rate of 23 cm3/10min.; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70ISO 2039-2
Tensile Strength, Yield 60.0 MPaISO 527-1/-2
Elongation at Break >= 50 %ISO 527-1/-2
Elongation at Yield 6.0 %ISO 527-1/-2
Tensile Modulus 2.30 GPaISO 527-1/-2
Flexural Strength 90.0 MPaISO 178
Flexural Modulus 2.40 GPaISO 178
Izod Impact, Notched (ISO) 60.0 kJ/m²
@Temperature 23.0 °C
ISO 180/4A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
IEC 60250
 3.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 29.0 kV/mmIEC 60243-1
Dissipation Factor 0.00066
@Frequency 100 Hz
IEC 60250
 0.0092
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 225 VIEC 60112
 250 - 399 VPLC 2; UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359-1/-2
Maximum Service Temperature, Air 125 °CBall Pressure Temperature; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 130 °CISO 75-1/-2
Vicat Softening Point 145 °C50°C/h 50N; ISO 306
UL RTI, Electrical 130 °C
@Thickness 0.750 mm
UL746B
 130 °C
@Thickness 3.00 mm
UL746B
UL RTI, Mechanical with Impact 125 °C
@Thickness 0.750 mm
UL746B
 130 °C
@Thickness 3.00 mm
UL746B
UL RTI, Mechanical without Impact 125 °C
@Thickness 0.750 mm
UL746B
 130 °C
@Thickness 3.00 mm
UL746B
Flammability, UL94 V-2
@Thickness 0.750 mm
IEC 60695-11-10
 V-2
@Thickness 1.60 mm
IEC 60695-11-10
Oxygen Index 26 %ISO 4589-1/-2
Glow Wire Ignition Temperature 825 °C
@Thickness 1.50 mm
IEC 60695-2-13
 875 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 800 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 89 %Light Transmittance; ASTM D1003
 
Descriptive Properties
Heat Stabilized or Stable to HeatYes
High Impact or Impact ModifiedYes
Injection MoldingYes
Light Stabilized or Stable to LightYes
Release AgentYes
TransparentYes
U.V. Stabilized or Stable to WeatherYes
Without FillersYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Altron™ PC Extruded, Unfilled, Polycarbonate
Covestro Makrolon® ET UV130 Polycarbonate
CENTROPLAST CENTROCARB Polycarbonate
Overview of materials for Polycarbonate, Molded
Mitsubishi Xantar® 22 UR Polycarbonate

PDSMEU546 / 31394

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.