MetalTek WCB UNS J13345 Cast Alloy Steel
Categories:
Metal
;
Ferrous Metal
;
Alloy Steel
;
AISI 4000 Series Steel
Material Notes:
General structural use.
Applications: Cylinders, rolls, hollow shafts.
Information provided by MetalTek
Key Words:
Cast UNS J13345; Cast Grade 9B; Cast ASTM A216; Wrought UNS G41300; Wrought Grade AISI 4130
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Hardness, Brinell
255
255
Tensile Strength, Ultimate
480
-
655
MPa
69600
-
95000
psi
Tensile Strength, Yield
>=
275
MPa
>=
39900
psi
Elongation at Break
>= 22 %
>= 22 %
Component Elements Properties
Metric
English
Comments
Carbon, C
<= 0.30 %
<= 0.30 %
Iron, Fe
>= 98.1 %
>= 98.1 %
As Balance
Manganese, Mn
<= 1.0 %
<= 1.0 %
Silicon, Si
<= 0.60 %
<= 0.60 %
Descriptive Properties
Heat Treatment
Quench & Temper
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
MetalTek WCC Cast 105-85 Alloy Steel
304 Stainless Steel
AISI Type S20910 Stainless Steel, annealed at 1120°C, water quenched
AISI 4130 Steel, normalized at 870°C (1600°F)
A. Schulman Diamond DIAMALOY 508 30% Glass Filled PC/Polyester Alloy, UV Stabilized
NMETEK114 / 18364
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.