MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Estane® 58246 Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Features: High stiffness grade with excellent chemical and oil resistance.

Uses: Flat Die/Cast Film Extrusion and Injection Molding.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccASTM D792
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 47 - 53
@Time 5.00 sec
ASTM D2240
Tensile Strength, Ultimate 64.1 MPaASTM D412
Elongation at Break 420 %ASTM D412
100% Modulus 0.0124 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0307 GPa
@Strain 300 %
ASTM D412
Tear Strength 180 pliTrouser; ASTM D470
Graves Tear Strength 800 pliDie C; ASTM D624
Tensile Set 12 %200% elongation; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 °CKofler
 170 °CDSC
Glass Transition Temp, Tg -20.0 °CDSC
 
Processing PropertiesOriginal ValueComments
Zone 1 199 °CExtrusion
Zone 2 204 °CExtrusion
Zone 3 210 °CExtrusion
Zone 4 216 °CExtrusion
Adapter Temperature 221 °C5, Extrusion
Die Temperature 221 °C6, Zone 1, Extrusion
 221 °CZone 2, Extrusion
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer
BASF Elastollan® C-85A Polyester Type Polyurethane Elastomer
Techmer ES HiFill® PVDF CF10 BK 10% Carbon Filled
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
BASF Elastollan® 1164D Polyether Type Polyurethane Elastomer

PNOVEON558 / 121449

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.