MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem ML3601U LLDPE Rotomolding Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade

Material Notes: The resin ML3601U is a linear low-density polyethylene, 1-hexene based, with excellent environmental stress cracking resistance and high impact strength. It contains long term UV8 stabilization and antioxidant additives. This resin is ideally suited for applications that require a higher mechanical performance. This resin was especially developed to produce rotomolded large tanks for water and chemical products storage, underground tanks, septic tanks, and manholes. This resin is recommended for rotational molding under conditions comparable to polyethylene resins with a similar melt index and density range. Oven temperature range: 180 to 350 ºC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.939 g/ccASTM-D1505
ESCR 100% Igepal® >= 1000 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
0.3 mm notched-plaques; ASTM-D1693
ESCR 10% Igepal® 145 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 3.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30.1 MPaASTM-D638
Tensile Strength, Yield 21.0 MPaASTM-D638
Elongation at Break >= 1000 %ASTM-D638
Elongation at Yield 14 %ASTM-D638
Flexural Modulus, 1% Secant 760 MPaASTM-D790
Impact Test 82.0 J
@Thickness 3.17 mm,
Temperature -40.0 °C
ARM
 228 J
@Thickness 6.34 mm,
Temperature -40.0 °C
ARM
 
Thermal PropertiesOriginal ValueComments
Melting Point 127 °CASTM-D3418
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °CASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 41.0 °CASTM-D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Bamberger Polymers Bapolene® 3042U Polyethylene, Rotational Molding Grade
Braskem ML4400N LLDPE Rotomolding Polyethylene
ExxonMobil LLP8450.31 Rotational Molding Resin
ExxonMobil LLP8555.24 Rotational Molding Resin

PBRAS875 / 106721

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.