MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Global EPP PA 6C OFN Cast Polyamide 6 + Blended Liquid Lubricant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of cast nylons may be altered to suit specific applications, and the performance of the basic polymer can be enhanced with the addition of various additives, fillers, lubricants and colorants.

Key characteristics:

  • Unequalled formulation options and profile range
  • Excellent mechanical, thermal and chemical resistance
  • Excellent PV and load bearing capabilities
  • Excellent wear and abrasion resistance
  • Good dimensional stability, largely free from internal stresses
  • FDA compliant grades available

A complex blended oil lubrication system, uniformly distributed throughout the product guarantees constant performance over the whole service life of this exceptional oil-loaded nylon. Excellent sliding frictional properties, abrasion resistance and stick/slip performance make this product a first choice for unlubricated moving parts.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³Test Method A; ISO 1183:1987
Water Absorption at Saturation 4.0 %4.0 %ISO 62:1999
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383ISO 868:2003
Tensile Strength at Break 75.0 MPa10900 psiSample Type 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 25 %>= 25 %Sample Type 1B, 50 mm/min; ISO 527-1/2:1993
Modulus of Elasticity 3.80 GPa551 ksiSample Type 1B, 50 mm/min; ISO 527-1/2:1993
Flexural Strength 95.0 MPa13800 psi1.5 mm/min; ISO 178:2001
Flexural Modulus 3.00 GPa435 ksi1.5 mm/min; ISO 178:2001
Compressive Strength 95.0 MPa13800 psiSample Type B, 5 mm/min; ISO 604:2002
Compressive Modulus 2.40 GPa348 ksiSample Type A, 1 mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 5.80 kJ/m²2.76 ft-lb/in²Sample Type A; ISO 180:2000
Coefficient of Friction, Dynamic 0.19
@Pressure 1.75 MPa
0.19
@Pressure 254 psi
31.4 m/min
K (wear) Factor 170 x 10-8 mm³/N-M
@Pressure 1.75 MPa
84.4 x 10-10 in³-min/ft-lb-hr
@Pressure 254 psi
31.4 m/min
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093:1980-01
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093:1980-01
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 60250:1969-01
 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 25.0 kV/mm635 kV/inIEC 60243-1:1998-01
Comparative Tracking Index 600 V600 VIEC 60112:2003-01
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-2:1999
Melting Point 220 °C428 °F
Maximum Service Temperature, Air 110 °C230 °FContinuous
 170 °C338 °FIntermittent
Minimum Service Temperature, Air -100 °C-148 °FIntermittent
 -40.0 °C-40.0 °FContinuous
Flammability, UL94 HBHBIEC 60695-11-10:2003-08
 
Descriptive Properties
ColorGreen and Yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Global EPP PA 6C Cast Polyamide 6
M Chemical GUARD DOG™ UV234 Light Absorber, Benzotriazole Derivative
M Chemical GUARD DOG™ UV360 Light Absorber
Global EPP PA 66E Extruded Polyamide 66
Global EPP PA 612 Copolymer Cast Polyamide 612

PGLOEPP05 / 79516

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.