MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess CS 7952 (28/779) Glass Fiber
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Fibers

Material Notes: CS 7952 (28/779)* is used for reinforcement of polypropylene. The normal coupling agents for polypropylene can be used.

Food contact grade, all sizing ingredients listed in EC/10/2011; Excellent mechanical strength in standard & impact modified PP grades; Good fiber integrity and Developed for application that require brilliant whiteness

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption <= 0.050 %
 
Descriptive Properties
Specifications0.7 percentSize content
 14 µmFiber Diameter
 4.5 mmAv. Fiber Length

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
R-Glass Fiber, Generic
Kingfa PA66-G50 50% Glass Fiber Reinforced PA66
Kingfa JH720 G50 50% Glass Fiber Reinforced PC
Glass Fiber Reinforced Concrete
Avient Polystrand ThermoPro™ IE6010 Unitape Unidirectional Polypropylene-Glass Composite

PLANY8655 / 209048

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.