MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lavergne VYPET VNT 630 FR PET 30% Glass Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced; Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

Material Notes: Vypet VNT 630 FR is a 30% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.

Features: Flame retardant; UL yellow card file E216152; Excellent strength and stiffness; Excellent dimensional stability
Typical Applications: Electrical parts; Appliances; Electronic applications

Information provided by Bieglo Gmbh for Lavergne Performance Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 2.00 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0090 cm/cm
@Thickness 2.00 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 145 MPa5 mm/min; ASTM D638
Flexural Strength 215 MPa1.3 mm/min; ASTM D790
Flexural Modulus 10200 MPa1.3 mm/min; ASTM D790
Izod Impact, Notched 90.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Strength 29.0 kV/mmASTM D149
Comparative Tracking Index 15 - 30 VUL746
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 228 °CASTM D648
Flammability, UL94 V-0
@Thickness 0.850 mm
 5VA
@Thickness 1.50 mm
 5VA
@Thickness 3.00 mm
Glow Wire Ignition Temperature 825 °CGWIT at 1.0 mm; IEC 60695-2-13
Glow Wire Flammability Index 960 °CGWFI at 1.0 mm; IEC 60695-2-13
 
Processing PropertiesOriginal ValueComments
Feed Temperature 260 - 270 °C
Middle Barrel Temperature 265 - 275 °C
Front Barrel Temperature 270 - 290 °C
Nozzle Temperature 275 - 295 °C
Melt Temperature 275 - 295 °C
Mold Temperature 95.0 - 120 °C
Injection Pressure 55.0 - 85.0 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RheTech Products GC30P200-01 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Cast Stainless Steel 17- 4, UNS J92150 (Compostion Spec)
Phillips Sumika Marlex® CHN-250 Polypropylene Talc-Filled Impact Copolymer
434 Stainless Steel annealed sheet
420 Stainless Steel

PLAVER909 / 150636

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.