MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MetalTek IN® 718 UNS N07718 Centri-Vac Nickel Cobalt Based Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Information provided by MetalTek

Key Words: Cast UNS N07718; AMS 5383 (investment casting); NACE MR0175
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.23 g/cc0.297 lb/in³Based on UNS number
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 860 MPa>= 125000 psi
Tensile Strength, Yield >= 760 MPa>= 110000 psi
Elongation at Break >= 5.0 %>= 5.0 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.020 - 0.080 %0.020 - 0.080 %
Cb + Ta 4.4 - 5.4 %4.4 - 5.4 %
Chromium, Cr 17 - 21 %17 - 21 %
Molybdenum, Mo 2.8 - 3.3 %2.8 - 3.3 %
Nickel, Ni 50 - 55 %50 - 55 %
 
Descriptive Properties
Heat TreatmentSol. Anneal & Age

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek IN® 909 Centri-Vac Nickel Cobalt Based Alloy
Elmet-Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
NiCoForm NiColoy® E Electroformed Nickel-Cobalt
Special Metals INCONEL® Alloy 718
MetalTek IN® 713 UNS N07713 Centri-Vac Nickel Cobalt Based Alloy

NMETEK147 / 18397

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.