MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Havoline® SAE 10W-30 Motor Oil
Categories: Fluid; Lubricant

Material Notes:

All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhibitor, and foam suppressant additives.

Havoline Motor Oils are recommended for all four-stroke gasoline engines used in passenger cars, light trucks, powerboats, motorcycles, and other mobile and stationary equipment. They are excellent for high-revving engines in small cars and light trucks. All grades are specially formulated for use in both new and high-mileage cars, and in turbocharged as well as normally aspirated engines. SAE 10W-30 is recommended for many older vehicles and a few late model cars and trucks, often those with larger 6-cylinder and V-8 and/or high performance engines. SAE 10W-30 provides improved fuel economy relative to heavier viscosity grades.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

CPS Number: 222190; MSDS Number: 8599

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 30.4 °
Viscosity 5800 cP
@Temperature -25.0 °C
Cold Crank
Viscosity Measurement 135Viscosity Index
Kinematic Viscosity at 40°C (104°F) 73.5 cSt
Kinematic Viscosity at 100°C (212°F) 10.8 cSt
Ash 0.90 %Sulfated Ash
 
Chemical PropertiesOriginal ValueComments
Total Base Number 7.6ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -35.0 °C
Flash Point 232 °C
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.094 %
Zinc, Zn 0.103 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Mobil 1 10W-30
ChevronTexaco Supreme SAE 10W-30 Motor Oil
Phillips 66 HD Fleet Supreme™ 10W-30 Engine Oil
Overview of materials for Nylon 6, 30% Glass Fiber Filled

WTEXA080 / 76959

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.