MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Conditioned)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled

Material Notes: Capron 8231G is a 14% glass fiber reinforced polyamide 6 molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also available in heat stabilized (Capron 8231G HS) and/or pigmented versions.

Capron 8231G is ideally suited for more demanding performance applications such as safety helmet parts, washers, gears, engine and motor parts, chutes, and higher temperature environments.

Data provided by Allied Signal.

Processing: Max. water content 0.16%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 250-280 degC (482-536 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics critical, a mold surface temperature of 80-95 degC (176-203 degF) is required. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/cc(Dry)
Linear Mold Shrinkage 0.0050 cm/cmASTM Data MD (Dry)
Linear Mold Shrinkage, Transverse 0.011 cm/cmISO Data (Dry)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 65.0 MPaASTM data at 5 mm/min.
Tensile Strength, Yield 70.0 MPaASTM value at 50 mm/min.
 72.0 MPaISO value at 50 mm/min.
Elongation at Break 8.5 %Nominal
 9.0 %ASTM, 5 mm/min
Elongation at Yield 5.6 %ISO Value at 50 mm/min.
 6.0 %ASTM Value at 50 mm/min.
Tensile Modulus 2.69 GPasame value from ASTM and ISO test.
Flexural Yield Strength 100 MPaASTM Data
Flexural Modulus 2.40 GPaASTM Data
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 400 VISO data
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C(Dry)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 275 °CSee Materials Notes
Mold Temperature 95.0 °CSee Materials Notes
Drying Temperature 85.0 °CSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry)
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Dry)
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Conditioned)
LyondellBasell Alathon® M6028 High Density Polyethylene
Overview of materials for Nylon 66, 10% Carbon Fiber Filled

PALC40 / 23834

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.