MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kolon KOCETAL® K900 Standard Grade Acetal Resin
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Very low viscosity grade.

Applications: Thin and large products.

Information provided by API-Kolon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
Moisture Absorption at Equilibrium 0.22 %60% RH; ASTM D570
Linear Mold Shrinkage 0.020 cm/cmASTM D955
Melt Flow 42 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80ASTM D785
Tensile Strength 64.0 MPaASTM D638
Elongation at Break 45 %ASTM D638
Flexural Strength 96.0 MPaASTM D790
Flexural Modulus 2700 MPaASTM D790
Izod Impact, Notched 50.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
Dielectric Constant 3.7ASTM D150
Dielectric Strength 19.0 kV/mmASTM D149
Dissipation Factor 0.0060
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 130 µm/m-°CASTM D696
Melting Point 166 °CASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 158 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °CASTM D648
Vicat Softening Point 162 °CASTM D1525
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer
Kolon Kocetal® K700 General Purpose Grade Acetal Copolymer
Mitsubishi Iupital® F20-03 Copolymer Acetal
Celanese Hostaform® C 52021 POM, Unfilled
Kolon KOCETAL® EL304 Toughened Grade Acetal Resin

PKOKZ907 / 122609

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.