MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECATEC PEI GF50 S296 CP/IP/OS V01 natural Polyetherimide, 50% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 50% Glass Fiber

Material Notes:
  • electrically insulating
  • inherent flame resistance
  • very good mechanical strength
  • continuous service temperature up to 150 °C
Target Industries:
  • automotive industry
  • mechanical engineering
  • oil and gas industry
  • safety engineering
  • sporting goods

Information provided by Ensinger Inc.

Vendors: Ensinger TECAPEI™ glass fiber reinforced shapes, made from ULTEM® PEI with Ensinger's proprietary extrusion techniques, provide superior tensile strength, rigidity, and dimensional stability for your most demanding PEI applications.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.90 g/cc
Filler Content 50 %Fiber volume
 50.0 %Fiber Volume
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 450 MPaISO 527-4
Modulus of Elasticity 24.0 GPaISO 527-4
Flexural Strength 570 MPaISO 14125
Flexural Modulus 26000 MPaISO 14125
Compressive Strength 670 MPaISO 14126
Compressive Modulus 27000 MPaISO 14126
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
CTE, linear, Transverse to Flow 10.0 µm/m-°C
Maximum Service Temperature, Air 180 °Clong term
 200 °Cshort term
Glass Transition Temp, Tg 217 °C
 
Processing PropertiesOriginal ValueComments
Drying Temperature 150 °C
Dry Time 4.00 - 6.00 hour
 
Descriptive Properties
Colornatural
General material information0.24 mmply thickness (consolidated)
 1000 mmMaterial widths
 1270 mmMaterial widths
 296 g/m²Fiber areal weight
 446 g/m²Areal weight finished product
 E glassFiber type
 US 7781Fiber architecture
Resin weight content (%)33.7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN8252 / 319180

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.