MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene® KR92828 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: Applications
PETROTHENE KR 92828 is a high molecular weight, high density polyethylene-based compound designed for use in jacketing, conduit or wire insulation. KR 92828 contains a carbon black content of 2.5%. Antioxidant has been added to ensure thermal stability during processing.

Processing Techniques
KR 92561, like other thermoplastic polyolefin compounds, can be extruded as wire and cable insulation using a conventional extruder. Below are suggested extrusion conditions for KR 92561. These conditions are intended as general guidelines only and are not optimum values, since manufacturing conditions, such as extruder type and size have an effect on processing of thermoplastic compounds.

This product is from the former Equistar product line.

Key Words: HDPE; Carbon Black 2.5 %.; Jacketing
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.955 g/ccASTM D1505
ESCR 10% Igepal® >= 1000 hourASTM D1693
Absorption Coefficient 440ASTM D3349
Carbon Black Loading 2.6 %
Melt Flow 0.15 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength at Break 4600 psiASTM D638
Tensile Strength, Yield 2800 psiASTM D638
Elongation at Break 800 %ASTM D638
Flexural Modulus, 1% Secant 110000 psiASTM D780
1% Secant Modulus 77000 psiASTM D638
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2.00e+17 ohm-cmASTM D257
Dielectric Constant 2.5
@Frequency 1e+6 Hz
ASTM D1531
Dielectric Strength 550 V/milASTM D149
Dissipation Factor 0.00020
@Frequency 1e+6 Hz
ASTM D1531
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Brittleness Temperature <= -76.0 °CF50; ASTM D746
 
Processing PropertiesOriginal ValueComments
Feed Temperature 300 - 325 °F
Zone 2 350 - 400 °F
Zone 3 375 - 400 °F
Zone 4-x 460 - 500 °F
Adapter Temperature 475 - 500 °F
Die Temperature 475 - 500 °F
Melt Temperature 475 - 500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SCG Chemicals EL-Lene™ H2001WC High Density Polyethylene Wire & Cable Grade
Braskem GD5150K HDPE High Density Extrusion Polyethylene
Dow HDPE 30460M High Density Polyethylene
Braskem GP5550BK HDPE High Density Extrusion Polyethylene
Global BM-3245-PC High Density Polyethylene, Pipe Extrusion Grade

PEQU0258 / 36692

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.