MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chi Mei Polylac® PA-716 ABS - High Flow  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: High flow, medium impact

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cmASTM D955
Melt Flow 3.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 38 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO-1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 112ASTM D785
Ball Indentation Hardness 98.0 MPaH358/30; ISO 2039-1
Tensile Strength at Break 35.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 46.0 MPa50 mm/min; ISO 527
Elongation at Break 10 %50 mm/min; ISO 527
Flexural Strength 65.0 MPa2 mm/min; ISO 178
Flexural Modulus 1.90 GPa2 mm/min; ISO 178
Izod Impact, Notched 2.22 J/cm
@Thickness 6.35 mm
ASTM D256
 2.49 J/cm
@Thickness 3.17 mm
ASTM D256
Izod Impact, Notched (ISO) 17.0 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) NBISO 180/1C
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 1.80 J/cm²ISO 179
Impact 13Impact Flexural Test Notched (KJ/m²)
 NBImpact Flexural Test Unnotched (KJ/m²)
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °Cunannealed; ISO 75
 97.0 °Cannealed; ISO 75
Vicat Softening Point 94.0 °C
@Load 5.00 kg
50°C/hr; ISO 306
 97.0 °C
@Load 5.00 kg
120°C/hr; ISO 306
 103 °C
@Load 1.00 kg
50°C/hr; ISO 306
 104 °C
@Load 1.00 kg
120°C/hr; ISO 306
Flammability, UL94 HB
@Thickness 1.59 mm
UL 94

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-737 ABS - High Flow
LG Chemical HF-350 ABS, High Flow, High Impact
Chi Mei Polylac® PA-746H ABS - High Flow
Chi Mei Polylac® PA-756H ABS - High Flow
Chi Mei Polylac® PA-746 ABS - High Flow

PCHI910 / 109398

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.