MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AdvanSix Capran® 1200MT Bi-Axially Oriented Nylon Film
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Capran® 1200MT is a bi-axially oriented nylon film. It is a versatile and robust film that satisfies many packaging needs, and has superior resistance to oils, fats, hydrocarbons, and many solvents. It is also microwavable, making it an excellent choice for lidding stock. 1200MT film has a metallized coating that provides an effective barrier to oxygen, helium, and water vapor.

Applications: message balloons as well as food packaging requiring high barrier.

Former Honeywell product; AdvanSix is a spin-off of Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0420 lb/in³Yield Density
Water Vapor Transmission 2.64 g/m²/day
@Temperature 37.8 °C
100%RH; ASTM F1249
Oxygen Transmission Rate 1.086 cc/m²/day77°F / 0% / RH; ASTM D3985
Thickness 0.480 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 60 - 90 %ASTM D882
Film Elongation at Break, TD 60 - 90 %ASTM D882
Secant Modulus, MD 2.41 - 3.93 GPaASTM D882
Secant Modulus, TD 2.482 - 3.59 GPaASTM D882
Coefficient of Friction 0.17 - 0.28film to stainless steel; ASTM D1894
 0.55 - 0.74film to film; ASTM D1894
Tear Strength Test 1100 - 1500graves tear, grams/mil (initial); ASTM D1004
Elmendorf Tear Strength, MD 10.42 - 16.67 g/mil
Film Tensile Strength at Break, MD 28000 - 40000 psiASTM D882
Film Tensile Strength at Break, TD 28000 - 40000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 1.6 - 2.5 %
@Treatment Temp. 160 °C,
Time 300 sec
ASTM D1204
Shrinkage, TD 0.20 - 0.70 %
@Treatment Temp. 160 °C,
Time 300 sec
ASTM D1204
 
Descriptive Properties
Helium Transition Ratemax 6 cc/100 in2/dayASTM 1434

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont™ Dartek® SF-502 Nylon 6,6 Super Formable Film, 76 µm Thickness
AdvanSix Capran® 1500 Clear Bi-Axially Oriented Nylon Film
AdvanSix Capran® 1200 Bi-Axially Oriented Nylon Film
AdvanSix Capran® 2500M M-Coated Bi-Axially Oriented Nylon Film
AdvanSix Capran® MT2500 Bi-Axially Oriented Nylon 6 Film

PALC006 / 23765

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.