MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper, UNS C61800, H02 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/2 Hard

Fabrication Properties: Good Suitability – Brazing, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Hot Formed; Fair Suitability – Capacity for Being Cold Worked, Soldering

Common Fabrication Processes: Blanking; Drawing; Hot forging; Hot Pressing

Typical uses: Bearing Liners; Bearings; Bushings; Pickling Hooks; Pump Impellers; Shafts; Tie Rods; Welding Rod; Marine Hardware

Applicable Specifications: Electrode – Welding AWS A5.6; Rod – Welding AWS A5.13, Welding AWS A5.7, Welding AWS A5.15; Wire – AWS A5.7, MILITARY MIL-W-6712

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.272 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 88
@Thickness 50.8 mm
 88
@Thickness 76.2 mm
 89
@Thickness 25.4 mm
Tensile Strength 80.0 ksi
@Thickness 76.2 mm
 83.0 ksi
@Thickness 50.8 mm
 85.0 ksi
@Thickness 25.4 mm
Tensile Strength, Yield 39.0 ksi
@Thickness 50.8 mm
0.5% Ext
 39.0 ksi
@Thickness 76.2 mm
0.5% Ext
 43.0 ksi
@Thickness 25.4 mm
0.5% Ext
Elongation at Break 23 %
@Thickness 25.4 mm
 25 %
@Thickness 50.8 mm
 28 %
@Thickness 76.2 mm
Tensile Modulus 17000 ksi
Modulus of Rigidity 6400 ksi
Poissons Ratio 0.33Calculated
Fatigue Strength 26000 psi
@Thickness 25.4 mm,
# of Cycles 1.00e+8
Machinability 40 %
Forgeability 50 %
Shear Strength 43.0 ksi
@Thickness 76.2 mm
 45.0 ksi
@Thickness 50.8 mm
 47.0 ksi
@Thickness 25.4 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000132 ohm-cm13% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 37.0 BTU-in/hr-ft²-°F
Melting Point 1904 - 1913 °F
Solidus 1904 °F
Liquidus 1913 °F
Annealing Point 1100 - 1200 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1400 - 1625 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 8.5 - 11 %
Copper, Cu 87.4 - 91 %As Balance
Iron, Fe 0.50 - 1.5 %
Lead, Pb <= 0.020 %
Silicon, Si <= 0.10 %
Zinc, Zn <= 0.020 %
 
Descriptive Properties
Cold Work (%)151 in
 152 in
 153 in
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC61800x1 / 293023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.