MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials HiDura™ ThermaPlus 24XLR8 NT0823 Nylon PA66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: HiDura ThermaPlus 24XLR8 NT0823 is a heat stabilized PA66 product designed for injection molding applications that is designed to maintain mechanical properties after extended exposure to temperatures up to 160 C.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDAM; ISO 1183
Water Absorption 1.9 %
@Temperature 23.0 °C,
Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 2.5 %
@Temperature 23.0 °C
DAM; ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 68.0 MPa50% RH; ISO 527-2
 78.0 MPaDAM; ISO 527-2
Elongation at Break 50 %DAM; ISO 527-2
 >= 50 %50% RH; ISO 527-2
Tensile Modulus 1000 MPa50% RH; ISO 527-2
 2600 MPaDAM; ISO 527-2
Flexural Strength 22.0 MPa50% RH; ISO 178
 86.0 MPaDAM; ISO 178
Flexural Modulus 900 MPa50% RH; ISO 178
 2800 MPaDAM; ISO 178
Poissons Ratio 0.30ISO 527-2
Izod Impact, Notched (ISO) 4.70 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 5.50 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 6.10 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 6.20 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 7.90 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 18.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
DAM; ISO 179/1eU
 NB
@Temperature -40.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 5.10 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 5.20 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 6.50 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 6.60 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 7.40 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 26.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 27.0 kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
 29.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 102 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 124 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 186 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °CUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature >= 260 °CInjection
 <= 280 °CInjection
Middle Barrel Temperature >= 270 °CInjection
 <= 285 °CInjection
Front Barrel Temperature >= 280 °CInjection
 <= 290 °CInjection
Nozzle Temperature >= 280 °CInjection
 <= 300 °CInjection
Melt Temperature >= 285 °CInjection
 <= 300 °CInjection
Mold Temperature >= 65.0 °CInjection
 <= 95.0 °CInjection
Drying Temperature <= 70.0 °CInjection
Dry Time >= 1.00 hourInjection
 <= 3.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
AppearanceNatural Color
FeaturesBalanced Stiffness/Toughness
 Chemical Resistant
 Excellent Processability
 Fast Molding Cycle
 Gasoline Resistant
 Good Flow
 Good Mold Release
 Good Toughness
 High Elongation
 High Heat Resistance
 High Tensile Strength
 Lubricated
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE8801 / 293370

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.