MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Innospec VISCOWAX® 334 EVA-Wax
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: CAS Number: 24937 - 78 - 8

VISCOWAX® 334 – high quality non-oxidised ethylene vinyl-acetate copolymer wax

Application:

  • Masterbatches
    • Carrier material and dispersing aid in pigment and additive concentrations
  • Paraffin compounding, candle industry
    • Improved elasticity
    • Improved burning behaviour if used as wick wax
  • Lacquers and Varnishes
    • Antisettling agent in metallic lacquers for pigment orientation
  • Hotmelts
    • Viscosity adjustment and improvement of flexibility and tack

Information provided by Innospec Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 - 0.950 g/ccDIN EN ISO 1183, C
Viscosity 300 - 500 cP
@Temperature 140 °C
DGF M-III 8
Molecular Weight 2300 g/molGPC
Vinyl Acetate Content 10 - 13 %FTIR
 
Mechanical PropertiesOriginal ValueComments
Penetration <= 7.0[10-1 mm], Needle; DGF M-III 9b
 
Thermal PropertiesOriginal ValueComments
Solidus 85.0 - 95.0 °CDGF M-III 4a
Dropping Point 96.0 - 102 °CDGF M-III 3
 
Descriptive Properties
AppearanceWhite
Type of deliveryFine grain

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Honeywell A-C® 400A EVA copolymer
Honeywell A-C® 405T EVA copolymer
Innospec VISCOWAX® 334 Granules EVA-Wax
ICO Polymers ICOFLO™ 510-5003 1000 Micron EVA Powder
Honeywell A-C® 645P EVA copolymer Oxidized

PINOS030 / 183473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.