MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ 5302 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: EMERGE™ ABS 5302 is a black, 20% glass-filled ABS which is suitable for use in a wide variety of internal structural component applications in the information technology market. This resin exhibits a property balance of low, rigidity, and dimensional stability.

Applications:
  • Information Technology Equipment and Consumer Electronics
  • Printer Internal Components
  • Structural Frames

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183B
Filler Content 20 %Glass; ISO 5630-B
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0035 - 0.0040 cm/cmISO 294-4
Melt Flow 1.6 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
 5.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 72.0 MPa
@Thickness 4.00 mm
50mm/min, injection molded, unannealed; ISO 527-2
Tensile Strength, Yield 72.0 MPa
@Thickness 4.00 mm
50mm/min, injection molded, unannealed; ISO 527-2
Elongation at Break 2.0 %
@Thickness 4.00 mm
50mm/min, injection molded, unannealed; ISO 527-2
Elongation at Yield 2.0 %
@Thickness 4.00 mm
50mm/min, injection molded, unannealed; ISO 527-2
Tensile Modulus 6.10 GPa1mm/min, 4mm injection molded, unannealed; ISO 527-2
Flexural Strength 115 MPa
@Thickness 4.00 mm
2mm/min, injection molded, unannealed; ISO 178
Flexural Modulus 6.20 GPa
@Thickness 4.00 mm
2mm/min, injection molded, unannealed; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²ISO 180/A
Charpy Impact, Notched 0.750 J/cm²
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
CTE, linear, Transverse to Flow 94.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 105 °Cunannealed; ISO 75-B
Deflection Temperature at 1.8 MPa (264 psi) 100 °Cunannealed; ISO 75-A
Vicat Softening Point 106 °C50°C / 50N; ISO 306-B50
 115 °C120°C / 10N; ISO 306-A120
Flammability, UL94 HB
@Thickness 1.00 - 2.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °C
Mold Temperature 20.0 - 60.0 °C
Drying Temperature 80.0 °C
Dry Time 3 - 4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Novodur® HD M203FC G3 Acrylonitrile Butadiene Styrene (ABS)
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
RTP Company RTP 605 Acrylonitrile Butadiene Styrene (ABS), Glass Fiber
A. Schulman Diamond ABS 1100
Chi Mei Kibilac® PW-978D ASA, High Heat

PZZDOW1330 / 30548

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.