MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Calcium Fluoride, CaF2 (Fluorite)
Categories: Ceramic; Halide

Material Notes: White cubic crystals or powder.

Hardness property values are typical of naturally occurring Fluorite. Actual hardness values will vary from sample to sample.

Key Words: CaF2
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 3.18 g/cc
a Lattice Constant 5.4638 Å
Formula Units/Cell (Z) 4
Molecular Weight 78.075 g/mol
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 139 - 152
Hardness, Vickers 175 - 200
Hardness, Mohs 4
Abrasive Hardness 5
Drilling Hardness 143
 
Electrical PropertiesOriginal ValueComments
Magnetic Susceptibility -0.0000280cm^3/mol
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 384.2 J/g
CTE, linear 19.5 µm/m-°C
Melting Point 1418 °C
Boiling Point 2533.4 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.434
@Wavelength 589.3 nm
η, Na
 
Descriptive Properties
CAS Number7789-75-5
ColorWhite
Crystal StructureCubicFluorite

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Thorium Oxide, ThO2 (Thorianite)
MV Labs CA500 CaF2 Calcium fluoride
Mateck Calcium Fluoride (CaF2)
MarkeTech Lutetium Aluminum Garnet:Cerium (LAG:Ce) Scintillator Crystal
Mateck Fused Silica UV-VIS Grade (SiO2)

EINOR0108 / 3237

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.