MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Polybilt™ Bitumen Modifier 101 Low Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: Polybilt 101 is compatible with a large variety of bitumens. For optimum results are preliminary study is recommended to determine the base bitumen grade and optimum Polybilt 101 content to achieve the desired end-use properties.
  • Boots binder softening point and decreases penetration.
  • Gives modified blends with excellent storage stability and handling characteristics.
  • Particularly recommended for easy mixing in less compatible bitumen.

Availability: Africa & Middle East, Asia Pacific and Europe

Additive:

  • Thermal Stabilizer: No
Applications:
  • Bitumen modifier

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.943 g/ccExxonMobil method
Viscosity 3100 cP
@Temperature 190 °C
ASTM D3236
Vinyl Acetate Content 14 %ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 201 °FPeak Melting Point; ExxonMobil method
Crystallization Temperature <= 170 °C
Vicat Softening Point 118 °FASTM D1525
 
Descriptive Properties
Blending Temperature160-170°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Concrete, 1-4 Dry
Lucobit Lucobit® 1210 Ethylene Copolymer Bitumen
Unipetrol 50/70 Road Bitumen
ExxonMobil Polybilt™ Bitumen Modifier 106 Low Density Polyethylene Resin
Unipetrol 160/220 Road Bitumen

PEX99139 / 175375

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.