MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ TE200 Polyurethane Reactive Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as wood, fiber reinforced plastic (FRP) and many other plastics to themselves, to metal and glass. Extrudable grade with fast set time, long open time ideal for bonding wood. Yields thin glue lines.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/cc
Brookfield Viscosity 3000 cPThermosel using spindle #27
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60
Tensile Strength at Break 27.6 MPaASTM D638 Die C
Elongation at Break 625 %ASTM D638 Die C
Tensile Modulus 9700 psiASMT D638 Die C
Shear Strength 620 psi
@Temperature 82.0 °C
Overlap, Maple
 650 psi
@Temperature 23.0 °C
Overlap, Polystyrene, Substrate Failure
 1250 psi
@Temperature 23.0 °C
Overlap, Polyacrylic, Substrate Failure
 1250 psi
@Temperature 23.0 °C
Overlap, ABS, Substrate Failure
 1550 psi
@Temperature 82.0 °C
Overlap, FRP
 1700 psi
@Temperature 23.0 °C
Overlap, FRP, Substrate Failure
 1950 psi
@Temperature 23.0 °C
Overlap, Maple
 2150 psi
@Temperature 23.0 °C
Overlap, PVC, Substrate Failure
 2200 psi
@Temperature 23.0 °C
Overlap, Polycarbonate, Substrate Failure
Peel Strength 9.00 pli180°, Polystyrene
 12.0 pliT-Peel, Initial
 31.0 pliT-Peel, Aged 71°C for 2 weeks, Substrate failure
 46.0 pli180°, Polyacrylic, Cotton duck failed during testing
 80.0 pli180°, FRP, Cotton duck failed during testing
 80.0 pli180°, ABS, Cotton duck failed during testing
 80.0 pli180°, PVC, Cotton duck failed during testing
 90.0 pli180°, Polycarbonate, Cotton duck failed during testing
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 minSet Time
 
Descriptive Properties
AppearanceWhite/Off-White

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Jet-Weld™ TE-200 Adhesive

PMM34760 / 169507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.