MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Baydur® 263 IMR RIM system
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Solid RIM

Material Notes: Characterization: Baydur 263 IMR is a black pigmented, two component, low-density, structural RIM (LD-SRIM) system.

Properties / Applications: Baydur 263 IMR is used in combination with glass reinforcement to mold automotive composite parts. The composite parts are produced by the open pour reaction injection molding process. The liquid resin mixture ’s low viscosity and long cream time allows it to fully permeate the glass reinforcement before reacting to form the solid crosslinked polymer. A variety of different fiberglasses can be used for reinforcement, such as: continuous roving glass mat, chopped strand glass mat, or with glass rovings utilizing a chopped glass fiber RIM machine. The system exhibits excellent flow, quick demold times, and outstanding mechanical properties. Typical composite applications include interior trim consoles, door trim panels, sunshades, and load floors. The Baydur 263 IMR system combines high strength and thermal properties, while still providing lighter weight than ABS, talc filled polypropylene (PP), or blow molded PP. Composites made with Baydur 263 IMR maintain dimensional stability under high heat and humidity conditions, even at thinner cross sections. Baydur 263 IMR can be poured into a mold to produce composite substrates separately, to be finished later with trim cover stock. Or, it can be poured directly behind trim cover stock, such as vinyl, fabric, or carpet, in a one-step process.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.450 g/cc300 g/m2 glass weight; ASTM D792
 0.550 g/cc600 g/m2 glass weight; ASTM D792
 1.05 g/ccPolyol (Component B)
 1.24 g/ccIsocyanate (Component A)
Viscosity 200 cPIsocyanate (Component A)
 1200 cPPolyol (Component B)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 20.0 MPa300 g/m2 glass weight; ASTM D638
 25.0 MPa600 g/m2 glass weight; ASTM D638
Flexural Strength 32.0 MPa300 g/m2 glass weight; ASTM D790
 40.0 MPa600 g/m2 glass weight; ASTM D790
Flexural Modulus 1350 MPa300 g/m2 glass weight; ASTM D790
 1600 MPa600 g/m2 glass weight; ASTM D790
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µin/in-°F600 g/m2 glass weight; ASTM D696
 20.0 µin/in-°F300 g/m2 glass weight; ASTM D696
Flash Point 145 °CPMCC, Polyol (Component B)
 199 °CPMCC, Isocyanate (Component A)
 
Processing PropertiesOriginal ValueComments
Mold Temperature 65.0 - 75.0 °C
Gel Time 0.750 min
 
Descriptive Properties
AppearanceBlack liquidPolyol (Component B)
 Dark brown liquidIsocyanate (Component A)
Content>31%NCO, Isocyanate (Component A)
Hydroxyl numberPolyol (Component B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayfill® EA 2204
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer
ExxonMobil Santoprene® 8211-55B100 Thermoplastic Elastomer
Covestro Baydur® 426 IMR RIM system
TIMCAL TIMREX® PP 10 Natural Flake Graphite

PCOVEST0079 / 201862

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.