MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lead-Base Babbitt Alloy 7, UNS L53581 (UNS L53585)
Categories: Metal; Nonferrous Metal; Lead Alloy

Material Notes: Composition reported for UNS L53585.

Key Words: Lead Base White Metal Bearing Alloy; ASTM B23 (8)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 10.2 g/ccCalculated
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 22
Tensile Strength, Ultimate 72.0 MPa
Elongation at Break 4.0 %in 50 mm
Compressive Yield Strength 24.5 MPa
Ultimate Compressive Strength 42.4 MPa
 
Thermal PropertiesOriginal ValueComments
Melting Point 240 - 268 °C
Solidus 240 °C
Liquidus 268 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.005 %
Antimony, Sb 14 - 16 %
Arsenic, As 0.30 - 0.60 %
Bismuth, Bi <= 0.10 %
Cadmium, Cd <= 0.05 %
Copper, Cu <= 0.50 %
Iron, Fe <= 0.10 %
Lead, Pb 75 %as remainder
Tin, Sn 9.3 - 10.7 %
Zinc, Zn <= 0.0050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lead-Base Babbitt Alloy 15, UNS L53620
Lead-Base Babbitt Alloy 7 (UNS L53465)
Lead-Base Babbitt Alloy 13, UNS L53346
Lead-Base Babbitt Alloy 8, UNS L53565
Lead-Tin Babbitt Alloy

MLB007 / 12207

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.