MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ravago Manufacturing Americas Hylac® HF224 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.

Information provided by Ravago.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cmASTM D955
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 22 g/10 min
@Load 3.80 kg,
Temperature 230 °C
Cond I; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 113ASTM D785
Tensile Strength, Yield 5200 psiASTM D638
Elongation at Break 46 %ASTM D638
Tensile Modulus 375000 psiASTM D638
Flexural Yield Strength 8200 psiASTM D790
Flexural Modulus 300000 psiASTM D790
Izod Impact, Notched 3.30 ft-lb/in0.25 in; ASTM D256
 3.70 ft-lb/in73°F, 0.125 in; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 51.0 µin/in-°F
@Temperature -40.0 - 176 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 208 °FUnannealed (0.250 in); ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 190 °FUnannealed (0.250 in); ASTM D648
Vicat Softening Point 221 °FASTM D1525
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 355 - 390 °F
Middle Barrel Temperature 390 - 430 °F
Front Barrel Temperature 420 - 455 °F
Nozzle Temperature 410 - 445 °F
Melt Temperature 465 °F
Mold Temperature 120 - 140 °F
Moisture Content <= 0.10 %
Injection Pressure 850 - 1000 psi
Back Pressure 70.0 - 140 psi
Shot Size 40 - 80 %
Screw Speed 50 - 90 rpm
 
Descriptive Properties
Holding Pressure710 to 850 psi
Injection RateSlow-Moderate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENTA030 / 36039

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.