MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Vistalon™ 805 EPDM Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Vistalon 805EPDM rubber is a medium Mooney viscosity, very high ethylene content, crystalline copolymer of ethylene and propylene with a narrow molecular weight distribution  This product is sold in crumb form. 

Availability:  Africa & Middle East, Europe, North America, Asia Pacific, Latin America.

Vistalon™ ethylene propylene diene (EPDM) rubber grades are used in a wide variety of applications in the automotive, consumer and industrial sectors. They deliver heat-resistant part performance and processing benefits that exceed those provided by natural and general-purpose rubbers.  Benefits:  Ozone and UV resistance, Water and polar fluid resistance, Heat resistance up to 175°C, Low temperature flexibility, Elastic properties under compression, Excellent physical properties at high filler loadings, Outstanding electrical insulation.

Information provided by ExxonMobil.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 33
@Temperature 125 °C
ML 1+4. Radial cavity, polymer remassed at 145°C; ASTM D1646
 
Descriptive Properties
Ethylene Content (%wt)78ASTM D3900B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker ELASTOSIL® LR 3003/90 A/B Liquid Silicone Rubber
Momentive Performance Materials Silopren™ LSR 3286/70 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set
Lanxess Keltan® 4577 EPDM Rubber
Lanxess Keltan® 4450 EPDM Rubber
Lanxess Keltan® 2650 EPDM Rubber

PEX98819 / 238204

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.