MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Zytel® 42A NC010 PA66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Unreinforced High Viscosity Polyamide 66

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³DAM; ISO 1183
Melt Density 1.01 g/cc
@Temperature >=262 °C
0.0365 lb/in³
@Temperature >=504 °F
Water Absorption 8.5 %
@Thickness 2.00 mm
8.5 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 2.60 %
@Thickness 2.00 mm
2.60 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Viscosity Number 300 cm³/g3.00 dl/gDAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 55.0 MPa7980 psi50% RH; ISO 527-1/-2
 83.0 MPa12000 psiDAM; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %50% RH; ISO 527-1/-2
 >= 50 %>= 50 %DAM; ISO 527-1/-2
Elongation at Yield 4.4 %4.4 %DAM; ISO 527-1/-2
 27 %27 %50% RH; ISO 527-1/-2
Tensile Modulus 1.30 GPa189 ksi50% RH; ISO 527-1/-2
 3.10 GPa450 ksiDAM; ISO 527-1/-2
Flexural Modulus 1.07 GPa155 ksi50% RH; ISO 178
 2.80 GPa406 ksiDAM; ISO 178
Poissons Ratio 0.370.37DAM; ISO 527-1/-2
 0.440.4450%RH; ISO 527-1/-2
Izod Impact, Notched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 180/1U
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 180/1U
Izod Impact, Unnotched (ISO)  6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 6.00 kJ/m²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 23.0 kJ/m²
@Temperature 23.0 °C
10.9 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 0.600 J/cm²
@Temperature 23.0 °C
2.86 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
Abrasion 3.53.5mm3, DAM; ISO 4649
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm50% RH; IEC 62631-3-1
 1.00e+15 ohm-cm1.00e+15 ohm-cmDAM; IEC 62631-3-1
Dielectric Constant  3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 4.3
@Frequency 100 Hz
4.3
@Frequency 100 Hz
DAM; IEC 62631-2-1
 10.3
@Frequency 100 Hz
10.3
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Dielectric Strength 30.5 kV/mm775 kV/inDAM; IEC 60243-1
Dissipation Factor  0.015
@Frequency 100 Hz
0.015
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.024
@Frequency 1e+6 Hz
0.024
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 0.075
@Frequency 1e+6 Hz
0.075
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 0.20
@Frequency 100 Hz
0.20
@Frequency 100 Hz
50% RH; IEC 62631-2-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 100 µm/m-°C55.6 µin/in-°FDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C55.6 µin/in-°FDAM; ISO 11359-1/-2
Specific Heat Capacity 2.79 J/g-°C
@Temperature >=262 °C
0.667 BTU/lb-°F
@Temperature >=504 °F
Melt
Thermal Conductivity 0.160 W/m-K
@Temperature >=262 °C
1.11 BTU-in/hr-ft²-°F
@Temperature >=504 °F
Melt
Melting Point 262 °C504 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FDAM; ISO 75-1/-2
Vicat Softening Point 244 °C471 °F50°C/h, 50N; ISO 306
Glass Transition Temp, Tg 70.0 °C158 °F10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
DAM; IEC 60695-11-10
Oxygen Index 28 %28 %DAM; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection
 290 °C554 °FInjection Optimum
Mold Temperature 50.0 - 90.0 °C122 - 194 °FInjection
 70.0 °C158 °FInjection Optimum
Ejection Temperature 190 °C374 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.050 %0.050 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiInjection
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Drying RecommendedyesInjection
Eff. thermal diffusivity7.00E-08 m²/s
FMVSS ClassSEISO 3795 (FMVSS 302)
Hold pressure time (s/mm)4Injection
Max. screw tangential speed (m/s)0.3Injection
Part Marking CodePA66ISO 11469
ProcessingCasting
 Coatable
 Film Extrusion
 Injection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
Regional AvailabilityNorth America
 South and Central America
Resin IdentificationPA66ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
Celanese Zytel® 103FHSA NC010 PA66
Celanese Zytel® 103FHS NC010 PA66
Celanese Zytel® 101 NC010 PA66
Asahi Kasei Leona® 1402SH Nylon 66

PDSX5314 / 197954

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.