MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aperam Nicrimphy® 601 Cold Rolled Strip
Categories: Metal; Ferrous Metal

Material Notes: Nicrimphy 601 is a nickel chromium alloy designed for applications requiring resistance to corrosion at high temperature. Nicrimphy 601 has also good resistance to aqueous corrosion. The high chromium content of Nicrimphy 601 increases its resistance against corrosion and substantial aluminium content provides excellent oxidation resistance at high temperatures. Nicrimphy 601 is used for: heat exchangers, industrial furnaces, thermoelectric safety (thermocouples), automotive industry (gasket, heat resistance cover in turbocharger, spark plug).

Information provided by Aperam

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.10 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 165Annealed
Tensile Strength 710 MPaAnnealed
Tensile Strength, Yield 310 MPaAnnealed
Elongation at Break 40 %Annealed
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000118 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.8 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.448 J/g-°C
Thermal Conductivity 11.2 W/m-K
Melting Point 1360 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 1.0 - 1.7 %
Chromium, Cr 21 - 25 %
Iron, Fe <= 18 %
Nickel, Ni 58 - 63 %
Titanium, Ti <= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NPERA035 / 194824

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.