MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay RHODASURF® BC-420 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: TRIDECYL ALCOHOL ETHOXYLATED

CAS: 78330-21-9

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODASURF BC-420 is a low foaming wetting agents for textile processing and alkaline spray cleaners. Emulsifiers for silicones and petroleum oils.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 - 0.938 g/ccRP-0549
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.50 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClear to cloudy, free flowing liquidRP-0064
Color<100APHA, RP-0134
Neutralization Number<0.5 mg KOH/gpH 7, RP-0343

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODASURF® CET 2 Surfactant
Solvay RHODASURF® BC-840 Surfactant
Solvay RHODASURF® ID/5 Surfactant
Solvay RHODASURF® ID 030 Surfactant
Solvay RHODASURF® DA-630 E Surfactant

WRHOD434 / 137665

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.