MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content between 25% and 34% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.41 - 1.58 g/ccAverage value: 1.48 g/cc Grade Count:38
Filler Content 30.0 %Average value: 30.0 % Grade Count:19
Water Absorption 0.0100 - 0.170 %Average value: 0.0508 % Grade Count:12
Additive Loading 25.0 - 30.0 %Average value: 28.8 % Grade Count:4
Viscosity 280000 - 400000 cP
@Temperature 310 - 310 °C
Average value: 340000 cP Grade Count:2
 280000 - 400000 cP
@Frequency 100 - 100 Hz
Average value: 340000 cP Grade Count:2
Linear Mold Shrinkage 0.000200 - 0.00600 cm/cmAverage value: 0.00142 cm/cm Grade Count:29
Linear Mold Shrinkage, Transverse 0.00150 - 0.00900 cm/cmAverage value: 0.00537 cm/cm Grade Count:11
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 98.0 - 110Average value: 104 Grade Count:3
Tensile Strength, Ultimate 46.9 - 236 MPaAverage value: 179 MPa Grade Count:36
 70.0 - 165 MPa
@Temperature 60.0 - 150 °C
Average value: 113 MPa Grade Count:1
Elongation at Break 0.500 - 3.00 %Average value: 1.19 % Grade Count:38
 0.900 - 1.80 %
@Temperature 60.0 - 150 °C
Average value: 1.40 % Grade Count:1
Modulus of Elasticity 4.83 - 33.8 GPaAverage value: 24.2 GPa Grade Count:29
 11.0 - 23.5 GPa
@Temperature 60.0 - 150 °C
Average value: 17.6 GPa Grade Count:1
Flexural Yield Strength 89.6 - 342 MPaAverage value: 259 MPa Grade Count:36
Flexural Modulus 8.00 - 30.0 GPaAverage value: 22.0 GPa Grade Count:36
Flexural Strain at Break 1.00 - 2.10 %Average value: 1.41 % Grade Count:9
Compressive Yield Strength 30.3 - 190 MPaAverage value: 129 MPa Grade Count:3
Izod Impact, Notched 0.310 - 2.51 J/cmAverage value: 0.632 J/cm Grade Count:20
Izod Impact, Unnotched 3.20 - 4.65 J/cmAverage value: 3.82 J/cm Grade Count:17
Izod Impact, Notched (ISO) 8.00 - 14.0 kJ/m²Average value: 10.2 kJ/m² Grade Count:3
 7.00 - 7.00 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 7.00 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 30.0 - 30.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 30.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 1.30 - 6.00 J/cm²Average value: 2.91 J/cm² Grade Count:7
Charpy Impact, Notched 0.160 - 0.800 J/cm²Average value: 0.495 J/cm² Grade Count:13
Coefficient of Friction 0.0800 - 0.290Average value: 0.196 Grade Count:6
Coefficient of Friction, Static 0.130 - 0.250Average value: 0.208 Grade Count:5
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0100 ohm-cm - 1e+05Average value: 1790 ohm-cm Grade Count:30
Surface Resistance 100 - 10000 ohmAverage value: 2390 ohm Grade Count:8
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 - 20.0 µm/m-°CAverage value: 12.1 µm/m-°C Grade Count:8
 5.00 - 20.0 µm/m-°C
@Temperature 100 - 200 °C
Average value: 12.5 µm/m-°C Grade Count:4
CTE, linear, Transverse to Flow 18.0 - 45.0 µm/m-°CAverage value: 38.3 µm/m-°C Grade Count:7
 100 - 110 µm/m-°C
@Temperature 100 - 200 °C
Average value: 103 µm/m-°C Grade Count:4
Melting Point 278 - 280 °CAverage value: 279 °C Grade Count:7
Deflection Temperature at 1.8 MPa (264 psi) 255 - 280 °CAverage value: 265 °C Grade Count:34
Flammability, UL94 V-0 - 5VBGrade Count:31
 
Processing PropertiesOriginal ValueComments
Processing Temperature 288 - 340 °CAverage value: 312 °C Grade Count:6
Melt Temperature 285 - 345 °CAverage value: 319 °C Grade Count:23
Mold Temperature 120 - 177 °CAverage value: 150 °C Grade Count:29
Drying Temperature 80.0 - 150 °CAverage value: 141 °C Grade Count:22
Moisture Content 0.0200 - 0.0400 %Average value: 0.0385 % Grade Count:13
Injection Pressure 30.0 - 124 MPaAverage value: 87.7 MPa Grade Count:18

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
Overview of materials for Polysulfone (PSU)
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

O4523 / 78346

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.