MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zoltek™ PX35 UD150 Uni-Directional Carbon Fabric
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK PX35 Stitch-Bonded Uni-Directional Carbon Fabrics are produced from ZOLTEK PX35 50K Continuous Tow Carbon Fiber. Unique fiber spreading techniques are utilized to obtain a wide range of UD fabric weights for a varied set of composite part applications. Quick composite part build-up is cost effectively achieved with the diverse weight range of low-cost carbon fabric products.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 210 micronsCured Thickness/Ply
 
Descriptive Properties
Fabric Component: 0° Carbon Zoltek PX35 50K (g/m2)158
Fabric Component: 90° Glass 34 dtex (g/m2)10
Fabric Component: Polyester Stitch 76 dtex (g/m2)6
Roll Length100 m
Roll Width30 cm-61cm-122cm
Stitch LengthA variety are available.
Stitch PatternA variety are available.
Total Fabric Weight (g/m2)182

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sinotek Materials Packing Carbon Fiber with Graphite
Sinotek Materials Packing Carbonized Fiber Braided
Carlisle 201LD Carbon-Carbon Composite
Zoltek™ PX35 Milled Carbon Fiber
E-Glass Fiber, Generic

ECZO801 / 232261

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.