MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AdvanSource Biomaterials ChronoPrene™ 40A Thermoplastic Rubber Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: ChronoPrene™ is a family of biocompatible thermoplastic elastomeric materials

ChronoPrene™ is a family of easy molding, high flow rubber, with excellent chemical resistance to alcohols, acids, and bases. ChronoPrene™ is offered as a translucent resin in a durometer hardness of 5 - 40 Shore A. The outstanding characteristic of this family of compounds is their ability to be injection molded at temperatures between 175ºC and 235ºC. The result is an injected molded part with very good surface smoothness and excellent elasticity.

ChronoPrene™ elastomeric resins are thermoplastic rubbers, which can be extruded or molded by standard thermoplastic processing equipment. Most traditional rubbers are thermosetting in nature, often making them difficult to compound, mold, and are not always biocompatible.

Information provided by AdvanSource Biomaterials Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 403 sec.; ASTM D2240
Tensile Strength, Ultimate 700 psiASTM D412
Elongation at Break 500 %ASTM D412
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 260 °FUpper stability limit
Mold Temperature 30.0 - 55.0 °FWarp-free parts
 175 - 235 °FMaximum surface smoothness and rubberiness
 
Descriptive Properties
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AdvanSource Biomaterials ChronoPrene™ 25A Thermoplastic Rubber Elastomer
ATI Allvac® Vasco® 316-L Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane
AdvanSource Biomaterials ChronoFlex® C 75D Biodurable Medical Grade Polyurethane
AdvanSource Biomaterials HydroMed™ D640 Permanently Lubricious Polyurethane Coating

PCARDI09 / 27933

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.