MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Fluorocarbon ETFE/ECTFE, Molded/Extruded
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Fluorocarbon ETFE/ECTFE, Molded/Extruded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.18 - 1.88 g/ccAverage value: 1.73 g/cc Grade Count:35
Water Absorption 0.00700 - 0.0300 %Average value: 0.0206 % Grade Count:13
Water Absorption at Saturation 0.0100 - 0.100 %Average value: 0.0775 % Grade Count:4
Particle Size 100 - 500 µmAverage value: 288 µm Grade Count:6
Water Vapor Transmission 12.92 - 12.92 g/m²/day
@Temperature 37.8 - 37.8 °C
Average value: 12.9 g/m²/day Grade Count:1
Thickness 1.00 - 2000 micronsAverage value: 872 microns Grade Count:12
Linear Mold Shrinkage 0.0180 - 0.0250 cm/cmAverage value: 0.0200 cm/cm Grade Count:7
Melt Flow 1.00 - 60.0 g/10 minAverage value: 14.4 g/10 min Grade Count:29
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 90.0 - 94.0Average value: 91.3 Grade Count:3
Hardness, Shore D 62.0 - 75.0Average value: 69.9 Grade Count:15
Tensile Strength, Ultimate 20.0 - 59.0 MPaAverage value: 41.5 MPa Grade Count:32
 4.55 - 50.0 MPa
@Temperature 40.0 - 200 °C
Average value: 23.2 MPa Grade Count:5
Tensile Strength, Yield 5.00 - 30.0 MPaAverage value: 17.0 MPa Grade Count:7
Elongation at Break 50.0 - 950 %Average value: 444 % Grade Count:34
 410 - 620 %
@Temperature 200 - 200 °C
Average value: 528 % Grade Count:5
Elongation at Yield 4.00 - 5.00 %Average value: 4.67 % Grade Count:3
Modulus of Elasticity 0.500 - 1.66 GPaAverage value: 1.48 GPa Grade Count:5
Flexural Yield Strength 24.0 - 48.3 MPaAverage value: 34.9 MPa Grade Count:9
 5.00 - 20.0 MPa
@Temperature 35.0 - 150 °C
Average value: 12.5 MPa Grade Count:5
Flexural Modulus 0.860 - 1.69 GPaAverage value: 1.11 GPa Grade Count:16
 0.100 - 0.900 GPa
@Temperature 30.0 - 120 °C
Average value: 0.369 GPa Grade Count:5
Compressive Yield Strength 8.00 - 38.0 MPaAverage value: 17.4 MPa Grade Count:11
Flex Crack Resistance 8500 - 600000Average value: 65500 Grade Count:19
Izod Impact, Notched 100 - 5340 J/cmGrade Count:14
 2.10 - 2.10 J/cm
@Temperature -40.0 - -40.0 °C
Average value: 2.10 J/cm Grade Count:2
 2.10 - 2.10 J/cm
@Thickness 3.20 - 3.20 mm
Average value: 2.10 J/cm Grade Count:2
Coefficient of Friction 0.0300 - 1.60Average value: 0.380 Grade Count:10
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 - 1.00e+17 ohm-cmAverage value: 7.88e+16 ohm-cm Grade Count:23
Surface Resistance 7000 - 1.00e+15 ohmAverage value: 5.58e+14 ohm Grade Count:9
Dielectric Constant 2.50 - 2.60Average value: 2.59 Grade Count:24
Dielectric Strength 14.0 - 197 kV/mmAverage value: 53.0 kV/mm Grade Count:25
Dissipation Factor 0.000600 - 0.0100Average value: 0.00409 Grade Count:16
Arc Resistance 120 - 122 secAverage value: 122 sec Grade Count:6
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 - 140 µm/m-°CAverage value: 103 µm/m-°C Grade Count:14
Specific Heat Capacity 0.962 - 1.26 J/g-°CAverage value: 1.18 J/g-°C Grade Count:8
Thermal Conductivity 0.150 - 0.216 W/m-KAverage value: 0.179 W/m-K Grade Count:3
 0.150 - 0.150 W/m-K
@Temperature 40.0 - 40.0 °C
Average value: 0.150 W/m-K Grade Count:2
Melting Point 180 - 280 °CAverage value: 246 °C Grade Count:33
Maximum Service Temperature, Air 149 - 180 °CAverage value: 151 °C Grade Count:32
Deflection Temperature at 0.46 MPa (66 psi) 82.0 - 115 °CAverage value: 94.6 °C Grade Count:7
Deflection Temperature at 1.8 MPa (264 psi) 62.0 - 85.0 °CAverage value: 68.3 °C Grade Count:9
Brittleness Temperature -125 - -76.0 °CAverage value: -111 °C Grade Count:7
Flammability, UL94 V-0Grade Count:14
Oxygen Index 30.0 - 52.0 %Average value: 36.2 % Grade Count:22
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 290 - 320 °CAverage value: 305 °C Grade Count:13
Melt Temperature 260 - 300 °CAverage value: 280 °C Grade Count:13
Mold Temperature 60.0 - 120 °CAverage value: 90.0 °C Grade Count:13
Injection Velocity 1.00 - 15.0 mm/secAverage value: 8.00 mm/sec Grade Count:13
Injection Pressure 50.0 - 120 MPaAverage value: 85.0 MPa Grade Count:13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
3M Scotch® FP-301 Heat Shrink Tubing
Overview of materials for High Density Polyethylene (HDPE), Extruded
Overview of materials for ECTFE Fluoropolymer

O1936 / 77921

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.