MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Du-Co Ceramics DC-16-L-3 Steatite
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.60 g/cc
Water Absorption 0.00 - 0.020 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 7.5
Tensile Strength, Ultimate 59.0 MPa
Flexural Strength 124 MPa
Compressive Strength 552 MPa
Impact Test 0.560 Junspecified impact test
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 5.5
@Frequency 1e+6 Hz
Dielectric Strength 9.10 kV/mm
Dissipation Factor 0.0050
@Frequency 1e+6 Hz
Dielectric Loss Index 0.028
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.39 µm/m-°C
@Temperature 20.0 - 650 °C
Thermal Conductivity 3.40 W/m-K
Maximum Service Temperature, Air 1000 °CSafe Operating Temp

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GBC Cerasil™ 223U Ceramic
California Fine Wire Stablohm 812 Chromium, Aluminum, and Iron Resistance Wire
Du-Co Ceramics CS-144-L-5 Steatite
Morgan Advanced Ceramics Frequentite 1000 Steatite
Morgan Advanced Ceramics Steatite 22 Steatite

CDUC02 / 778

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.