MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond EP21TDC-4ND Two component, highly flexibilized epoxy for bonding, sealing and coating
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond EP21TDC-4ND is a two component, very flexible epoxy system for high performance bonding, sealing and coating with a non-drip consistency. It has a one to four mix ratio by weight. EP21TDC-4ND has a room temperature cure that can be accelerated by adding heat. The best cure schedule is overnight at room temperature followed by 3-4 hours at 150-200°F. A peculiar feature of this product is that straight heat curing results in a product that is slightly softer (Shore A 60), than the one with the optimum cure (Shore A 75). The cured system has a peel strength greater than 30 pli and an elongation of over 200%. EP21TDC-4ND bonds well to a wide variety of metals, plastics and especially rubbers. In fact, it may adhere well to untreated rubber materials such as neoprene, nitrile, SBR and occasionally EPDM rubber compounds; materials that normally require time consuming surface preparation. The cured system has solid electrical insulation properties along with good chemical resistance to oils and water. The epoxy has good resistance to aggressive thermal cycling along with great resistance to mechanical shock and vibration. EP21TDC-4ND has an exceptionally long open time greater than 90 minutes. It has a service temperature range of -100°F to +250°F, low temperature serviceability. It is widely used in OEM, electrical, electronic, repair and maintenance type applications.

Product Advantages:

  • Convenient mixing: non-critical, one to four mix ratio, by weight, available in premeasured kits
  • Smooth paste viscosity; non-drip type system
  • Versatile cure schedules: ambient temperature cures or faster elevated temperature cures
  • High peel strength and exceptionally robust resistance to thermal cycling and shock
  • Bonds especially well to rubber including neoprene, nitrile, SBR and occasionally EPDM
  • Outstanding resistance to thermal cycling

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75 - 80using the optimum cure schedule
Tensile Strength at Break >= 3000 psi
@Temperature 23.9 °C
Elongation at Break <= 200 %
Tensile Modulus 100000 - 150000 psi
@Temperature 23.9 °C
Shear Strength >= 850 psi
@Temperature 23.9 °C
Al/Al, Tensile lap
Peel Strength >= 30.0 pliT-peel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 - 130 µm/m-°C
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 - 4.00 hour
@Temperature 93.3 °C
 4.00 - 5.00 hour
@Temperature 23.9 °C
 12.0 hour
@Temperature 23.9 °C
Followed by 2-3 hours at 150-200°F (Optimum Cure Schedule)
Pot Life >= 90 min100 gram mass
Shelf Life 12.0 Month
@Temperature 23.9 °C
in original unopened containers
 
Descriptive Properties
Mixing Ratio (A to B)1:4by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP21TDC-4 Two Component, Highly Flexible Epoxy System
Armacell Monarch® F-03091 (Black) Pure EPDM Foam
Saint-Gobain COHRlastic® 440S Silicone Solid/High Temp Silicone Adhesive Pressure Sensitive Tape
Armacell Ensolite™ EF0 EPDM crushed foam
Armacell Monarch® F-03092 (Black) EPDM Foam

PMASTB320 / 149567

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.