MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Alathon® M5363 High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Applications
ALATHON L 4912 is a high molecular weight, high density copolymer with a broad molecular weight distribution. This resin provides excellent stiffness and a good balance of film properties as a single component or in blends. It is designed to process well on grooved feed or smooth bore equipment. L 4912 may be used in a variety of applications such as liners, over-wrap, multi-wall sheeting, merchandise and produce bags.

Regulatory Status
L 4912 meets the requirements of the Food and Drug Administration, regulation 21 CFR 177.1520. This regulation allows the use of olefin polymer in “...articles or components of articles intended for use in contact with food.” Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing L 4912 can only be made when the processing conditions, equipment and end use are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.953 g/ccASTM D1505
Melt Flow 6.5 g/10 minASTM D1238
Spiral Flow 9.50 inSpiral channel (0.625” insert) with injection pressure of 1000 psi at 440°F.; Equistar Test
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67ASTM D2240
Tensile Strength at Break 3250 psiASTM D638
Tensile Strength, Yield 4110 psiCrosshead Speed 2 in/min; ASTM D638
Elongation at Yield 7.3 %Crosshead Speed 2 in/min; ASTM D638
Flexural Modulus, 1% Secant 181000 psiCrosshead Speed 0.5 in/min; ASTM D790
2% Secant Modulus 151000 psiCrosshead Speed 0.5 in/min; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °CASTM D648
Vicat Softening Point 127 °CASTM D1525
Brittleness Temperature <= -76.0 °CF50; ASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Ateva® 1807EG Medical Grade EVA
ExxonMobil Escorene® LD-760 High EVA Compounding Resin
Innospec FLEXAREN® 18000 EVA-Copolymer
ICO Polymers ICOFLO™ 510-5003 1000 Micron EVA Powder
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer

PEQU0738 / 37207

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.