MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
H.C. Starck NRC® Tantalum (UNS R05200)
Categories: Metal; Nonferrous Metal; Refractory Metal; Pure Element

Material Notes: Applications: High strength and excellent corrosion resistance make tantalum ideal for use in the manufacture and repair of chemical process equipment and heat exchangers. Other uses are rupture discs, cathode plates, heat shielding, ordnance, sputtering and medical applications.

Forms Available: Foil, Sheet, Plate, Welded Tubing, Rod, Wire and Bar.

Metallurgical Characteristics: Material is single-phase tantalum. Stress relieve at 1500°F, re-crystallize at 1900°F.

Information provided by H.C. Starck.

Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 16.6 g/cc
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 180.95
Atomic Number 73
Thermal Neutron Cross Section 21.3 barns/atom
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 25 - 65hardness as annealed, typical
Hardness, Vickers 80 - 120hardness as annealed, typical
Tensile Strength >= 23.2 ksi
@Temperature 249 °C
 >= 25.4 ksi
@Temperature 199 °C
 >= 29.0 ksi
@Temperature 98.9 °C
 >= 30.0 ksi
@Temperature 21.1 °C
Tensile Strength, Ultimate 35.0 - 45.0 ksi
@Temperature 20.0 °C
typical
Tensile Strength, Yield 20.0 - 30.0 ksi
@Temperature 20.0 °C
typical
 >= 10.1 ksi
@Strain 0.2 %,
Temperature 249 °C
 >= 11.6 ksi
@Strain 0.2 %,
Temperature 199 °C
 >= 14.5 ksi
@Strain 0.2 %,
Temperature 98.9 °C
 >= 20.0 ksi
@Strain 0.2 %,
Temperature 21.1 °C
Elongation at Break >= 10 %
@Temperature 199 °C
 >= 15 %
@Temperature 98.9 °C
 >= 20 %
@Temperature 21.1 °C
Modulus of Elasticity 27000 ksi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.0000147 ohm-cm
@Temperature 0.000 - 100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.60 µin/in-°F
@Temperature 20.0 - 500 °C
Specific Heat Capacity 0.0336 BTU/lb-°F
@Temperature 100 °C
Thermal Conductivity 384 BTU-in/hr-ft²-°F
@Temperature 20.0 - 100 °C
Melting Point 3017 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.0050 %
Hydrogen, H <= 0.0010 %
Iron, Fe <= 0.0050 %
Molybdenum, Mo <= 0.020 %
Nickel, Ni <= 0.0050 %
Niobium, Nb (Columbium, Cb) <= 0.030 %
Nitrogen, N <= 0.0050 %
Oxygen, O <= 0.010 %
Silicon, Si <= 0.0010 %
Tantalum, Ta >= 99.884 %balance
Titanium, Ti <= 0.0040 %
Tungsten, W <= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tantalum, UNS R05200
Tantalum, Ta; Annealed
Tantalum, Ta; Cold Worked
Tantalum, UNS R05400
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade

NHCST930 / 130820

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.