MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI 1522 Steel Composition Spec (UNS G15220)
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Key Words: UNS G15220
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³Typical Carbon Steel
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell >= 149>= 149
Elongation at Break >= 20 %>= 20 %in 2 in. (50 mm)
Reduction of Area >= 42 %>= 42 %
Modulus of Elasticity 200 GPa29000 ksiTypical Carbon Steel
Poissons Ratio 0.290.29Typical Carbon Steel
Shear Modulus 78.0 GPa11300 ksiTypical Carbon Steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000170 ohm-cm0.0000170 ohm-cmTypical Carbon Steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C6.67 µin/in-°FTypical Carbon Steel
Specific Heat Capacity 0.470 J/g-°C0.112 BTU/lb-°FTypical Carbon Steel
Thermal Conductivity 52.0 W/m-K361 BTU-in/hr-ft²-°FTypical Carbon Steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.18 - 0.24 %0.18 - 0.24 %
Iron, Fe 98.27 - 98.72 %98.27 - 98.72 %As Balance
Manganese, Mn 1.1 - 1.4 %1.1 - 1.4 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1524 Steel, Hot Rolled Bar (UNS G15240)
AISI 8620 Steel, annealed 13 mm (0.5 in.) round
SAE 1518 Carbon Steel, Composition Spec
ASTM A36 Steel, plate
AISI 1020 Steel, normalized at 870°C (1600°F)

M1522 / 100211

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.