MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hapco ULTRALLOY 108 White Polyurethane Liquid
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Liquid

Material Notes: A series of general purpose Liquid Molding Compounds. This product turns a natural white but is available pigmented white for extra brightness. Both versions are available in an 8.5 minute or 25 minute gel time.:
  • General purpose
  • 1:1 by weight
  • Available in 2 speeds

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D-4669
Viscosity 250 - 350 cPASTM D-4878
Linear Mold Shrinkage 0.0010 - 0.0030 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ASTM D-2240
Tensile Strength 7700 psiASTM D-638
Elongation at Break 8.6 %ASTM D-638
Modulus of Elasticity 145 ksiASTM D-638
Flexural Strength 11900 psiASTM D-790
Flexural Modulus 314 ksiASTM D-790
Izod Impact, Notched 0.810 ft-lb/inASTM D-256
Izod Impact, Unnotched >= 8.93 ft-lb/inASTM D-256
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 70.0 °CASTM D-648
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 - 6.00 hour
@Thickness 3.17 mm
Demold
Gel Time 25.0 min
@Load 0.100 kg
ASTM D-2971
 
Descriptive Properties
Color (cured)pigmented white
Mix Ratio100:100Weight
 100:120Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHAPCO179 / 317238

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.